Halina Krawiec, Janusz Lelito
The influence of heat treatment parameters such as the annealing time and austempering temperature on the microstructure, tribological properties and corrosion resistance of ductile iron have been investigated. It has been revealed that the scratch depth of cast iron samples increases with the extension of the isothermal annealing time (from 30 to 120 min) and the austempering temperature (from 280 ◦C to 430 ◦C), while the hardness value decreases. A low value of the scratch depth and a high hardness at low values of the austempering temperature and short isothermal annealing time is related to the presence of martensite. Moreover, the presence of a martensite phase has a beneficial influence on the corrosion resistance of austempered ductile iron.
@article{8bc32476-ac7b-4f8a-8c7a-0f81c19e4ac2,
title={Influence of Heat Treatment Parameters of Austempered Ductile Iron on the Microstructure, Corrosion and Tribological Properties},
author={Halina Krawiec and Janusz Lelito},
year={2023},
language={English}
}TY - JOUR TI - Influence of Heat Treatment Parameters of Austempered Ductile Iron on the Microstructure, Corrosion and Tribological Properties AU - Halina Krawiec AU - Janusz Lelito PY - 2023 LA - English ER -
Xiaomei Li
The ever growing demands for high strength aluminium alloys in the aerospace industry have greatly enhanced the development of alloy chemistry and the
J.D. Kordatos, G. Fourlaris
The welding of duplex stainless steels, specifically SAF 2205, presents challenges in achieving a balanced microstructure consisting of both ferrite a
Thomas G. Digges, Samuel J. Rosenberg
This monograph presents a comprehensive exploration of the heat treatment processes and the resulting properties of iron and steel, critical materials
George E. Hicho, John H. Smith
A metallurgical evaluation was conducted to determine if selected castings of 17-4PH stainless steel had been properly heat treated as required by SAE
G.E. Hicho, W.J. Boettinger
This study examines a mishap section and other selected sections made from 17-7 precipitation hardening stainless steel, revealing an unusually large
G.E.Hicho, W.J.Boettinger
We have examined the failed or "mishap" section, and other selected sections made from 17-7 precipitation hardening stainless steel, and have conclude