Extracting aluminum from aluminum alloys in AlCl3−NaCl molten salts was investigated. Al coating was deposited on the copper cathode by the method of direct current deposition using aluminum alloys as anode. The purity of the deposited aluminum is about 99.7% with the energy consumption of 3−9 kW·h per kg Al, and the current efficiency is 44%−64% when the deposition process is carried out under 100 mA/cm2 for 4 h at 170 °C. The effects of experimental parameters, such as molar ratio of AlCl3 to NaCl, cathodic current density and electrolysis time, on the current efficiency were studied. The molar ratio of AlCl3 to NaCl has little effect on the current efficiency, and the increase of deposition temperature is beneficial to the increase of current efficiency. However, the increase of current density or electrolysis time results in the decrease of current efficiency. The decrease of current efficiency is mainly related to the formation of dendritic or powder deposit of aluminum which is easy to fall into the electrolyte.
@article{c7b2c2c1-96c2-487d-9093-12f6d7aead55,
title={Current efficiency of recycling aluminum},
author={Jun-li XU and Jing ZHANG},
year={2026},
language={en}
}TY - JOUR TI - Current efficiency of recycling aluminum AU - Jun-li XU AU - Jing ZHANG PY - 2026 LA - en ER -
TUNGKY SUBROTO, ALEXIS MIROUX
Numerical process simulation is increasingly used to optimize direct-chill (DC) casting of aluminum alloys, yet crack-susceptibility predictions depen
Unknown, Unknown
This chapter discusses metal casting processes, highlighting the diversity and common characteristics among them. The objective is to elucidate the fu
Unknown, Unknown
This study focuses on the fundamental characteristics of solid iron, which is predominantly composed of iron atoms and provides a basis for understand
Ir. Méshac KIME ILUNGA
Ce document traite des procédés métallurgiques spéciaux, en mettant particulièrement l'accent sur l'extraction liquide-liquide, un processus mis au po
Copper solvent extraction units at large hydrometallurgical plants face constraints in metal recovery, phase disengagement, and reagent consumption, d